LiNiCoMnO2 (Ni:Co:Mn=5:2:3, NCM523) Powder for High Power Li-ion Battery Cathode 200g/bottle - Lib-LNCM523
LiNiCoMnO2 (Ni:Co:Mn=5:2:3, NCM523) Powder for High Power Li-ion Battery Cathode 200g/bottle - Lib-LNCM523
Minimum Order: $20 (equipment), $100 (crystals)
97 in stock
SKU: : \Lib-LNCM523
Couldn't load pickup availability

LiNiCoMnO2 (Lithium Nickel Manganese Cobalt Oxide) powder for Li-ion power battery cathode 200g/bottle (Ni:Co:Mn=5:2:3, NCM523 or NMC532)
Specification
| Item | Description | Testing Method |
| D10 (μm) | ≤ 5.0 | Laser Particle Size Analyzer |
| D50 (μm) | 10.0-14.0 | |
| D90 (μm) | ≥25.0 | |
| Appearance | Dark brown powder, atmospheric stability | |
| Elements Proportions | Ni:Co:Mn = 5:2:3 | |
| Ni+Co+Mn (%) | ≥58 | Volumetry |
| Li (%) | 7.00-8.00 | Atomic Absorption Spectroscopy Inductively Coupled Plasma |
| Fe (%) | ≤0.01 | |
| Na (%) | ≤0.03 | |
| Cu (%) | ≤0.005 | |
| H2O (%) | ≤0.05 | Coulometric KF Titrator |
| PH | ≤ 11.50 | PH Tester |
| H2O (%) | ≤ 0.1 | Moisture Analyzer |
| Specific Surface Area (m2/g) | 0.20-0.40 | BET Analyzer |
| Specific Capacity (mAh/g) [1st cycle] | 153-158 | 0.2C, 4.2-2.7 V vs Li/Li+, Half Cell |
| Columbia Efficiency (%) [1st cycle] | ≥85% | |
Note: MTI does not manufacture this product, and only sell the small quantity to research for development for new generation battery. If you need a larger quantity or have the question for IP, we will forward your inquiry to the producer.
| XRD |
![]() |
![]() |
Application Notes:
- Please click to see Procedure for Preparing Anode & Cathode Electrode Slurry.
- Please keep the powder in vacuum box to avoid moisture.
- Please bake the powder in a vacuum oven at 120 - 150 °C before making slurry and coating to ensure max. capacity.
Related Products
|
Vacuum Storage Box |
Powder Milling & Mixer |
Electrode Coaters |
Battery Research Equipment |
Other Battery Powders |