Single Crystal Powder of LiNiCoMnO2 (Ni:Co:Mn=8:1:1, NCM811) with LiNbO3 Coating for Li-Ion Battery Cathode, 200g/bottle - Lib-LNCM811-SCLN
Single Crystal Powder of LiNiCoMnO2 (Ni:Co:Mn=8:1:1, NCM811) with LiNbO3 Coating for Li-Ion Battery Cathode, 200g/bottle - Lib-LNCM811-SCLN
Minimum Order: $20 (equipment), $100 (crystals)
19 in stock
SKU: : \Lib-LNCM811-SCLN
Couldn't load pickup availability

Single Crystal powder of LiNiCoMnO2 (Lithium Nickel Manganese Cobalt Oxide, Ni:Co:Mn=8:1:1, NCM811 or NMC811) with surface coating of LiNbO3 is a excellent cathode powder with high stability for solid-state lithium-ion battery application.
Specification
| Properties | Item | Typical Value |
|
Chemical Composition |
Ni (mol%) | 82.1% |
| Co (mol%) | 12.0% | |
| Mn (mol%) | 5.9% | |
|
Size Distribution |
D10 (μm) | 2.1 |
| D50 (μm) | 3.9 | |
| D90 (μm) | 7.0 | |
| Specific Surface Area (m2/g) | BET | 0.58 |
| Tap Density (g/cm³) | 3.53 | |
| Residual |
Li2CO3 (wt%) |
0.113 |
| LiOH (wt%) | 0.173 | |
|
|
0.1 C | 210 mAh/g |
|
Columbic Efficiency (first cycle) |
0.1C | 92.4% |
|
Specific Capacity (mAh/g) for all-solid-state battery |
0.1C (Discharge) Columbic Efficiency |
200 mAh/g 80% |
|
Note |
MTI does not manufacture this product, and only sell the small quantity to research for development for new generation battery. If you need a larger quantity or have a question for IP, we will forward your inquiry to the producer. | |
- Please click to see Procedure for Preparing Anode & Cathode Electrode Slurry.
- Please keep the powder in the vacuum box to avoid moisture.
- Please bake the powder in a vacuum oven at 120 - 150 °C before making slurry and coating to ensure max. capacity.
- The product is for research only, not supply for large quantity,