Skip to product information
1 of 1

Precursor Powder of NCMOH811 for High Capacity NCM Cathode Powder 200g/bottle - EQ-Lib-PNCM811

Precursor Powder of NCMOH811 for High Capacity NCM Cathode Powder 200g/bottle - EQ-Lib-PNCM811

14 in stock

Regular price $399.00 USD
Regular price Sale price $399.00 USD
Sale Email for Lead Time

SKU: : \Lib-PNCM811

View full details

Lib-PNCM811 is the precursor powder of NCMOH811 for High Capacity NCM Cathode Powder at your own composition.
There are 200 grams in one bottle
Note:  You must mix the precursor with LiOH. H2O and calcine the mixed powder at 750- 790oC before use

Specification                                                       

 Package

  200g/bottle in a vacuumed bag

 Composition

  NCMOH811

 Configuration

 Sphere

 Particle size  distribution

D105.36 μm
D5011 μm
D9018.6 μm

 Magnetic substance

102 ppd

 Tap Density

≥1.74 g/cm^3

 Water Content 

wt%0.5

 PH value 

~ 8.38

 

Mian Element

   Required Content (mol)

Ratio (Ni:Co: Mn)

 

Li

0

0

 

Ni

47.7247

7.994

 

Co

6.3195

1.059

 

Mn

5.6562

0.947

 

Impurity 

Requiredppm

Typicalppm

 

Ca

300

16

 

Cu

50

1

 

Fe

100

15

 

Mg

300

2

 

Na

500

229

 

Zn

100

121

 

SO4

5000

3000

  Note

MTI does not manufacture this product, and only sell the small quantity to research for development for new generation battery.   If you need a larger quantity or have a question for IP, we will forward your inquiry to the producer.



Application Notes
:
  1. Please click to see Procedure for Preparing Anode & Cathode Electrode Slurry.
  2. Please keep the powder in a vacuum box to avoid moisture.
  3. Please bake the powder in a vacuum oven at 120 - 150 °C before making slurry and coating to ensure max. capacity.

Related Products

Vacuum Storage Box
laboratory mill and mixer    
Powder Milling & Mixer
 
Electrode Coaters

Battery Research Equipment

Other Battery Powders

Solid Electrolyte
Manufacturer Part Number: